Khoom taw qhia
High Precision TI6AL4V Titanium Alloy Tubes yog titanium alloy qib raws li ASTM system. Nws cov tshuaj muaj pes tsawg leeg yog Ti-6Al-4V (titanium{17}}6 aluminium-4 vanadium). Nws yog ib qho + dual-theem titanium alloy thiab yog lub zog siab titanium alloy nrog lub ntiaj teb loj tshaj plaws ntau lawm ntim thiab ntau yam kev siv, suav txog ntau dua 50% ntawm tag nrho cov titanium alloy noj. Qhov tseem ceeb, nws yog tubing tsim los ntawm kev tsim cov txheej txheem siv Ti-6Al-4V alloy ua raw khoom. Nws tau txais lub zog tshwj xeeb thiab zoo heev corrosion kuj ntawm GR5 alloy, thaum tseem muaj cov micron-theem seem qhov raug thiab tsis tshua muaj siab saum npoo zoo, ua rau nws yog ib qho tseem ceeb rau kev ua tiav lub teeb yuag thiab kev ntseeg siab hauv cov khoom siv high-end.
Tshuaj muaj pes tsawg leeg
| Cov ntsiab lus | Al | V | Fe | C | N | H | O | Ti |
|---|---|---|---|---|---|---|---|---|
| Scope ntawm Standard | 5.5–6.75 | 3.5–4.5 | Tsawg dua lossis sib npaug li 0.40 | Tsawg dua lossis sib npaug li 0.10 | Tsawg dua los yog sib npaug li 0.05 | Tsawg dua lossis sib npaug li 0.015 | Tsawg dua los yog sib npaug li 0.20 | Tseem tshuav |
| Hom Kev Tswj | 6.0–6.3 | 4.0–4.2 | Tsawg dua lossis sib npaug li 0.25 | Tsawg dua los yog sib npaug li 0.05 | Tsawg dua lossis sib npaug li 0.03 | Tsawg dua lossis sib npaug li 0.010 | Tsawg dua lossis sib npaug li 0.15 | Tseem tshuav |
- Al (Aluminium): Ib qho -theem-stabilizing lub ntsiab uas muab cov tshuaj tiv thaiv kom muaj zog thiab txhim kho lub zog thiab elastic modulus ntawm ob chav tsev kub thiab kub.
- V (Vanadium): A -theem-stabilizing lub caij uas txhim kho ductility thiab processability thiab suppresses nkig nag lossis daus ntawm ₂ theem.
- O (Oxygen): Ib qho khoom nruab nrab uas ua rau kom muaj zog tab sis txo cov ductility; nyob rau hauv precision raj, nws yog nruj me ntsis tswj ntawm tsawg dua los yog sib npaug zos rau 0.15% kom paub meej txias- ua hauj lwm formability.
- H (Hydrogen): Ib qho teeb meem uas tuaj yeem ua rau hydrogen embrittlement yooj yim; Lub tshuab nqus tsev annealing tuaj yeem txo cov ntsiab lus hydrogen kom tsawg dua lossis sib npaug li 0.010%.
Mechanical thiab Physical Properties
Cov khoom ntawm GR5 siab-precision titanium alloy raj yog ze ze rau lawv qhov kev tsim khoom (xws li, annealed lossis txias- ua haujlwm).
- Mechanical Properties (Chaw Kub Kub, Hom Annealed Condition)
- Tensile Strength: Ntau dua lossis sib npaug ntawm 895 MPa. Qee cov khoom siv siab - precision tuaj yeem ncav cuag tshaj 1000 MPa.
- Tawm Zog: Ntau dua lossis sib npaug rau 828 MPa.
- Elongation Tom Qab Fracture: Ntau dua lossis sib npaug li 10%, qhia tias cov khoom khaws cia qee qhov kev sib tw thaum tuav lub zog siab.
- Modulus ntawm Elasticity: Kwv yees li 110 GPa.
- Physical thiab Chemical Properties
- Qhov ntom ntom: kwv yees li 4.43 g / cm³, uas tsuas yog kwv yees li 60% ntawm cov hlau, muab qhov hnyav hnyav -txuag qhov zoo.
- Corrosion Resistance: Exhibits tsis tshua muaj corrosion kuj nyob rau hauv seawater, chlorides, ntau yam acids, thiab organic solvents, deb tshaj ntawm stainless hlau.
- Biocompatibility: Tsis yog- tshuaj lom thiab hypoallergenic, nrog kev muaj peev xwm osseointegration zoo, ua rau nws tsim nyog rau kev cog qoob loo.
Technical Tolerances
"High precision" tshwj xeeb yog cuam tshuam rau hauv qhov nruj heev qhov ntev thiab qhov zoo ntawm qhov chaw, uas yog qhov tseem ceeb ntawm qhov sib txawv ntawm cov raj no sib nrug los ntawm cov raj titanium.
| Kev ntsuas qhov tseeb | Tus nqi tsim nyog rau Standard Titanium Tubes | Cov Lus Qhia Tshwj Xeeb rau GR5 Siab -Titanium Tubes Precision |
|---|---|---|
| Outer Diameter Tolerance | ± 1% lossis dav | ± 0.1 hli, Precision qib mus txog ± 0.05 hli |
| Phab ntsa Thickness kam rau ua | ± 12.5% ntawm nominal phab ntsa thickness | ± 0.05 hli |
| Sab hauv phab ntsa Roughness (Ra) | - | Tsawg dua lossis sib npaug li 0.2μm, Sab hauv phab ntsa yog du thiab tsis muaj burrs |
| Concentricity yuam kev | - | Tsawg dua lossis sib npaug li 0.01mm / m (Rau Ntxiv -Long Pipes) |
| Qhov Loj | - | OD: 0.3mm - 101.6mm; WT: 0.05mm - 5mm (Customizable) |
Core Strengths
High Precision TI6AL4V Titanium Alloy Tubes
Siab zog + Tsawg ceev
Lub zog tensile Ntau dua lossis sib npaug ntawm 895 MPa, nrog qhov ceev ntawm tsuas yog 4.43 g / cm³; nws lub zog tshwj xeeb tshaj li ntawm 304/316 stainless hlau (7.93 g / cm³) thiab siab - lub zog steel. Nyob rau hauv cov xwm txheej sib npaug, cov yeeb nkab phab ntsa tuaj yeem ua nyias, txo qhov hnyav ntawm 30-40%.
Zoo heev Corrosion Resistance
Qhov saum npoo ua rau nws tus kheej-passivation los ua ib daim duab ntom ntom TiO₂ oxide, muab kev tiv thaiv corrosion los ntawm seawater, chloride ions, feem ntau cov kua qaub (tshwj tsis yog hydrofluoric acid, kub concentrated hydrochloric acid, thiab sulfuric acid), alkalis, thiab ntsev tov. Nws tiv taus pitting thiab crevice corrosion, thiab nws lub neej kev pab cuam nyob rau hauv marine ib puag ncig thiab tshuaj lom neeg tshaj tawm yog 5-10 lub sij hawm ntev tshaj li ntawm stainless hlau. Nws ua rau tsis muaj paug corrosion los ntawm- cov khoom, ua rau nws haum rau cov khoom noj, tshuaj, thiab siab - cov kua purity.
High Dimensional Accuracy thiab Consistency
Sab nraud txoj kab uas hla, phab ntsa thickness, thiab roundness tolerances ntawm precision txias-raws raj raws li precision{1}}qib cov qauv, xyuas kom meej sib dhos interchangeability. Cov hlab ntaws zoo heev phab ntsa thickness uniformity, ruaj khov siab-cov kabmob muaj peev xwm, thiab tsis muaj qhov chaw tsis muaj zog. Nrog siab inner bore precision, lawv yog haum rau siv raws li hydraulic lub tog raj kheej chim, valve spool tes tsho, thiab precision kua passages.
Zoo heev Low-Tsub Ua Haujlwm
Tsis muaj ductile - mus rau - nkig hloov kub, nws tuav zoo toughness txawm nyob rau ntawm -196℃(kua nitrogen), ua rau nws haum rau cryogenic engineering thiab aerospace kua hydrogen / kua oxygen piping systems.
Biocompatibility
Ti-6Al-4V ELI (Ntxiv-Low Interstitial) yog cov khoom siv rau kev cog qoob loo kho mob; industrial-qib GR5 tubing tuaj yeem siv rau hauv cov ntawv thov cuam tshuam nrog cov khoom noj thiab tshuaj.
Tsis yog-magnetic
Titanium alloys tsis yog- cov khoom sib nqus thiab tsim nyog siv rau hauv electromagnetic - qhov chaw muaj kev cuam tshuam (cov khoom siv kho mob, cov cuab yeej hluav taws xob precision, thiab cov tshuab sib nqus).
Cov cheeb tsam tseem ceeb ntawm daim ntawv thov
1 Aerospace
- Aircraft hydraulic thiab roj kab
- Cav ducts thiab ib puag ncig tswj kab ke
- Rocket propellant hloov kab (kua hydrogen / kua oxygen)
- Satellite structural tubing
2 Offshore Engineering thiab Naval Vessels
- Seawater piping thiab condenser raj rau nuclear submarines thiab naval nkoj
- Risers thiab dej- cais cov casings rau offshore roj drilling platforms
- Piping rau seawater desalination nroj tsuag
- Lub cev muaj zog rau cov khoom siv tshawb nrhiav dej hiav txwv
3 Chemical and Energy Industries
- Kub exchangers thiab condenser raj (ASTM B338)
- Piping rau chlor-alkali kev lag luam thiab PTA cov nroj tsuag
- Cov kav dej pab rau cov tshuab hluav taws xob nuclear
- Cov cuab yeej downhole thiab roj zoo casing
4 Automotive thiab kev sib tw
- Sib xeem khiav cov kav dej thiab cov mufflers (lub teeb yuag + siab -kub resistant)
- Ncua tseg system tubing thiab yob tawb
- Nres system kab
- Motorcycle aftermarket tubing
5 Kev Kho Mob thiab Pharmaceutical
- Cov qauv tubing rau cov khoom siv kho mob (cov cuab yeej phais, orthopedic sab nraud fixation thav duab)
- Tubing rau kev thauj cov kua tshuaj (siab purity, tsis muaj corrosion thiab paug)
- Tubing rau cov khoom siv kom tsis muaj menyuam
6 Precision Machinery thiab Hydraulic
- Hydraulic cylinder chim (precision-qib bores sab hauv)
- Pneumatic Cheebtsam lub tog raj kheej
- Precision ntsuas bushings thiab valve spools
- Tsheb kauj vab ncej raj (Gr5/Gr9 titanium thav duab- siab- qauv kawg)
7 Kev Ua Si thiab Leisure
- Titanium alloy tsheb kauj vab ncej thiab diav rawg
- Golf qws ncej
- Hiking ncej thiab lub tsev pheeb suab ntaub
- Diving khoom tubing
Cov khoom tso tawm




txog peb lub tuam txhab

peb yog leej twg?
Ib - nres Titanium Processing Parts Factory hauv Suav teb
Peb Baoji Reliab Hlau Khoom Co., Ltd tau tsim nyob rau hauv xyoo 2014, nyob rau hauv lub npe nrov 'Tuam Tshoj Titanium Valley--BAOJI', nyob rau hauv lub muaj zog R & D muaj peev xwm thiab kev loj hlob tsis tu ncua, peb cov khoom tseem ceeb muaj xws li titanium & titanium alloy bars / rods, daim hlau, raj, forgings, fasteners & machined qhov chaw, thiab cov khoom siv zuag qhia tag nrho.
Peb tau dhau Daim Ntawv Pov Thawj Zoo ntawm ISO 9001-2015, aiming rau kev txaus siab ntawm cov neeg siv khoom sib txawv thov.
siab zoo
Khoom siv Advanced
Pab neeg tshaj lij
Ib -Stop Solution
siab zoo
Professional thiab Rigorous Manufacturing txheej txheem.
cov cuab yeej siv siab heev
Peb muaj lub xeev- ntawm-- cov khoom siv kos duab.
pab neeg tshaj lij
Kev mob siab rau thiab muaj lub luag haujlwm muag thiab tom qab- pab pawg muag khoom.
thoob ntiaj teb shipping
Ib qho yooj yim thiab yooj yim Shipping System.
Peb cov ntawv pov thawj thiab cov khoom siv kuaj

tiv tauj peb
E-mail:garychen3215@hotmail.com
Chaw nyob: No.35, Baoti Rd, Baoji nroog, Shaanxi Province, Suav
Hu rau: Mr. Gary Chen
Xov tooj: +86-917-8883215
Txawb/WhatsApp: +86 13092900605
Cim npe nrov: Tuam Tshoj siab precision ti6al4v titanium alloy raj manufacturers, lwm tus neeg, Hoobkas