Txhais Txog Gr5 Titanium seamless kav
Gr5 Titanium seamless kav yog tsim los ntawm Ti-6Al-4V (titanium-6-aluminium-4-vanadium) alloy thiab yog ib qho ntawm feem ntau siv titanium alloy raj hauv kev lag luam. GR5 yog ib qho - titanium alloy thiab raug suav hais tias yog "tus neeg ua haujlwm" ntawm titanium alloys vim nws qhov kev ua tau zoo tag nrho.
Nws yog lub ntiaj teb feem ntau siv thiab ntau yam seamless raj ua los ntawm ib qho + ob-theem cua sov- kho tau titanium alloy. Nrog lub zog siab, lub teeb yuag, zoo heev corrosion kuj, thiab zoo weldability thiab formability raws li nws cov txiaj ntsig zoo, nws yog qhov tsim nyog rau kev thov hauv aerospace, marine, chemical, kho mob, thiab high -kawg cov khoom lag luam.
Tshuaj muaj pes tsawg leeg
| Cov ntsiab lus | Standard Range |
Muaj nuj nqi |
|---|---|---|
| Ti |
Cov ntsiab lus seem |
Lub hauv paus ntsiab lus |
| Al | 5.5%–6.75% |
-stabilized, txhim kho lub zog, tiv thaiv tshav kub, thiab nkag siab |
| V | 3.5%–4.5% |
-stabilization; txhim kho ductility, weldability, thiab tshav kub kho hardenability |
| O | Tsawg dua lossis sib npaug li 0.20% (Standard); Tsawg dua lossis sib npaug li 0.13% (ELI) |
Interstitial ntxiv dag zog; tswj cov pa oxygen kom ntseeg tau tias muaj zog |
| N | Tsawg dua lossis sib npaug li 0.05% |
Interstitial impurities: nruj me ntsis tswj kom tsis txhob embrittlement |
| C | Tsawg dua lossis sib npaug li 0.08% |
impurities, cuam tshuam ductility |
| H | Tsawg dua lossis sib npaug li 0.015% |
nruj me ntsis tswj hydrogen kom tiv thaiv hydrogen embrittlement |
Kaum Properties ntawm Titanium
① Tsawg ceev, siab tshwj xeeb lub zog
② Zoo heev corrosion kuj
③ Ua haujlwm kub zoo
④ Kev ua haujlwm kub tsis zoo
⑤ Muaj zog Anti damping kev ua tau zoo
⑥ Tsis yog - sib nqus, Tsis yog - lom
⑦ Me me thermal conduction coefficient
⑧ Tsawg modules ntawm elasticity
⑨ Lub tshuab nqus tsev
⑩ Tensile zog ze rau lub zog tawm los
Mechanical Properties
|
Kev ntsuas kev ua haujlwm |
Yam tsawg kawg nkaus |
Tus nqi |
|---|---|---|
|
Lub zog tensile |
Ntau dua lossis sib npaug li 895 MPa | 930 ~ 970 MPa |
|
Yield zog |
Ntau dua lossis sib npaug li 828 MPa | 880 ~ 930 MPa |
|
Elongation |
Ntau dua lossis sib npaug li 10% | 12 ~ 14% |
|
Hla -sectional txo piv |
Ntau dua lossis sib npaug li 25% | 30 ~ 35% |
| Hardness (HRC) | 30 ~ 36 | 34 ~ 38 |
Specifications ntawm Gr5 Titanium seamless kav
1. Qhov Loj (Ntawm Diameter × Phab Ntsa Thickness × Length)
Sab nrauv (OD): Φ10mm-Φ200mm (tus qauv: Φ10-Φ108), customizable mus txog Φ300mm
Phab ntsa Thickness (WT): 1 mm–20 mm (tus qauv: 1–8 mm), nyias-walled Tsawg dua los yog sib npaug li 0.8 mm, tuab-walled Ntau dua los yog sib npaug li 15 mm
Ntev: 1000-6000 hli, ruaj ntev / random ntev, tuaj yeem txiav / chamfered / threaded
2. Tolerances (qib Precision)
Sab nraud txoj kab uas hla: ± 0.05-± 0.1 hli
Phab ntsa Thickness: ± 0.05-± 0.1 hli
Kev Ncaj Ncees: Tsawg dua lossis sib npaug li 0.5 mm / m
3. Nto tiav
Pickled thiab ci (tus qauv kev lag luam), sandblasted, txhuam, iav polished, anodized (xim xim)
Cov khoom nthuav qhia ntawm Gr5 Titanium seamless kav




tiv tauj peb
E-mail:garychen3215@hotmail.com
Chaw nyob: No.35, Baoti Rd, Baoji nroog, Shaanxi Province, Suav
Hu rau: Mr. Gary Chen
Xov tooj: +86-917-8883215
Txawb/WhatsApp: +86 13092900605
Cim npe nrov: gr5 titanium seamless kav, Tuam Tshoj gr5 titanium seamless kav manufacturers, lwm tus neeg, Hoobkas