Qhia txog qhov zoo ntawm Titanium alloy tsheb kauj vab chainring
Piv rau cov tsoos aluminium alloy, steel, lossis carbon fiber chainrings, titanium alloy chainrings muaj cov txiaj ntsig zoo hauv qab no:
- Qhov hnyav hnyav: Titanium alloy muaj qhov ntom ntawm kwv yees li 4.51 g / cm³, hnyav dua li aluminium alloy me ntsis (2.7 g / cm³), tab sis nws lub zog yog 2-3 npaug ntawm aluminium alloy.
- Ultra-High Strength thiab Durability: Lub zog tensile ntawm titanium alloy tuaj yeem ncav cuag 900-1100 MPa, deb tshaj li ntawm aluminium alloy (300-500 MPa), ua rau cov hniav tsis tshua muaj deformation lossis tawg.
- Kev qaug zog zoo heev: Nyob rau lub sijhawm ntev -, siab - zaus pedaling cyclic kev nyuaj siab, lub neej qaug zog ntawm titanium alloy yog 3-5 npaug ntawm aluminium alloy, ua rau nws tsim nyog rau kev nce toj siab lossis kev sib tw scenarios.
- Natural Corrosion Resistance: A dense oxide layer forms on the surface of titanium, providing resistance to corrosion from rain, sweat, and salt without the need for additional plating, resulting in a lifespan more than twice that of aluminum alloy chainrings.
- Cov yam ntxwv zoo damping: Lub elastic modulus ntawm titanium alloy yog ze rau ntawm cov hlau, uas tuaj yeem nqus tau qee qhov kev vibrations, txhim kho kev caij tsheb thiab txo cov suab nrov resonance.
Mainstream titanium alloy cov ntaub ntawv thiab cov txheej txheem ntawm titanium alloy tsheb kauj vab chainring
Common Alloy Hom:
- Ti-6Al-4V: Cov khoom siv chainring feem ntau, ua tiav qhov sib npaug ntawm lub zog siab thiab tawv los ntawm "kev kho kev daws teeb meem + kev laus" txheej txheem, tsim rau kev sib koom ua ke lossis CNC machining.
- Ti-6Al-4V ELI: Ib qho ultra-low interstitial impurity version nrog purity siab dua, feem ntau yog siv rau kev sib tw-qib chainrings qhov hnyav hnyav yog xav tau.
- Titanium alloy (piv txwv li, Ti-3Al-2.5V): Muab cov yas zoo dua, haum rau kev tsim cov hlua khi, thiab muaj cov khoom ua haujlwm txias, tab sis kim dua.
Core Manufacturing Txheej Txheem:
- Integral Forging: Titanium alloy blanks yog forged ntawm qhov kub thiab txias thiab tom qab ntawd precision machined siv CNC tshuab. Qhov no ua rau muaj cov qauv denser thiab pom lub zog thiab qaug zog ua haujlwm.
- CNC Integrated Machining: Cov khoom yog ncaj qha milled los ntawm titanium alloy daim hlau, ua tiav ib tug precision ntawm ± 0.02mm, haum rau complex hollowed -tawm designs rau poob phaus.
- Kev kho deg:
- Daim iav Polishing: Raws li qhia hauv koj daim duab, daim iav -zoo li tiav tiav los ntawm ntau txoj kev sib tsoo, txhim kho kev zoo nkauj thiab txo cov saw hlau.
- Sandblasting / Txhuam Txhuam: Tsim cov matte lossis textured nto, nkaum khawb thaum khaws cov xim hlau zoo nkauj.
- Anodizing: Tso cai rau kev tsim cov xim oxide txheej xws li kub thiab xiav, muab ob qho tib si zoo nkauj thiab tiv thaiv - cov khoom xeb.
Kev ua tau zoo thiab siv tau cov xwm txheej ntawm Titanium alloy tsheb kauj vab chainring
- Kev sib tw- qib kev tsheb kauj vab: Qhov hnyav txo tau txhim kho kev hloov pauv hluav taws xob thaum nce toj thiab sprinting, ua rau lawv zoo tagnrho rau cov neeg caij tsheb kauj vab uas nrhiav kev ua tau zoo tshaj plaws.
- Ntev -kev ncua deb ntawm kev caij tsheb kauj vab: Kev qaug zog zoo dua thiab ua haujlwm ntev txo qhov zaus ntawm kev saib xyuas thaum caij tsheb ntev.
- Tawm ntawm - txoj kev tsheb kauj vab: Lub zog siab tuaj yeem tiv taus qhov cuam tshuam ntawm cov struts struts, thiab corrosion kuj ua rau lawv haum rau hnyav ib puag ncig xws li los nag thiab av nkos.
Cov ntaub ntawv tseem ceeb ntawm kev ua tau zoo ntawm Titanium alloy tsheb kauj vab chainring
Cov khoom siv tseem ceeb ntawm titanium alloys (noj cov feem ntau siv Ti-6Al-4V ua piv txwv) deb tshaj cov tsoos txhuas alloy chainrings:
- Tensile zog: 900-1100 MPa (siab-kawg aluminium alloys tsuas yog 300-500 MPa)
- Yield zog: 860-1030 MPa (txhuas alloys yog kwv yees li 270-450 MPa)
- Kev qaug zog lub neej: 3-5 zaug ntev dua li txhuas alloy chainrings, tsawg dua rau cov hniav deformation los yog tawg nyob rau hauv siab - zaus pedaling cyclic stress
- Elastic modulus: Kwv yees li 110 GPa (ze rau cov hlau, ntau dua li 70 GPa ntawm aluminium alloys), zoo dua tuaj yeem nqus pedaling vibrations thiab txo cov saw resonance.
Cov khoom qhia ntawm Titanium alloy tsheb kauj vab chainring
Titanium alloy tsheb kauj vab chainring






Hais txog peb lub tuam txhab

Ib - nres Titanium Cov Khoom Lag Luam Hauv Tuam Tshoj
Baoji Reliab Hlau Khoom Co., Ltd yog cov chaw tsim khoom thiab chaw muag khoom ntawm titanium zeb cov khoom thiab cov khoom siv nickel, zirconium. Nrog kev tswj xyuas zoo, peb cov khoom ua tau raws li tus qauv thoob ntiaj teb xws li ASTM, ASME, AMS, JIS, DIN, TOCT, peb cov khoom tseem ceeb suav nrog cov tuav / pas nrig, daim hlau / ntawv, raj, xov hlau, forgings rings, anodes, fasteners thiab CNC machined qhov chaw.
Tau ntau tshaj 12 xyoos, Baoji Reliab Hlau Khoom tau loj hlob los ua ib qho ntawm cov chaw muag khoom ruaj khov rau aerospace-qib titanium thiab kev kho mob- qib titanium cov khoom lag luam hauv Suav teb.
tiv tauj peb li cas
E-mail:garychen3215@hotmail.com
Chaw nyob: No.35, Baoti Rd, Baoji nroog, Shaanxi Province, Suav
Hu rau: Mr. Gary Chen
Xov tooj: +86-917-8883215
Txawb/WhatsApp: +86 13092900605
Cov lus nug nquag
Q: Qhov no Titanium alloy tsheb kauj vab chainring tau tsim li cas?
A: Briefly speaking, Titanium alloy bicycle chainring was hot-forged==>CNC milled==>polished.
Q: Koj puas tuaj yeem ua LOGO ntawm Titanium alloy tsheb kauj vab chainring?
A: Peb tuaj yeem laser engraving cov neeg siv khoom logo dawb.
Q: MOQ ntawm Titanium alloy tsheb kauj vab chainring yog dab tsi?
A: Peb MOQ ntawm Titanium alloy tsheb kauj vab chainring yog 10 pcs.
Cim npe nrov: titanium alloy tsheb kauj vab chainring, Tuam Tshoj titanium alloy tsheb kauj vab chainring manufacturers, lwm tus neeg, Hoobkas