Qeb 23 Kev Kho Mob Titanium Nqes
video
Qeb 23 Kev Kho Mob Titanium Nqes

Qeb 23 Kev Kho Mob Titanium Nqes

Hom: Titanium kho mob, cog hniav, kho hniav
Cov Khoom Siv Qib: Gr5, Ti6al4V Eli, Gr23.
Nto: polished, zom, machined
Tshuag loj: Dia 1.0 hli ~ sia150mm * ntev3000mm
Xa kev nug
Hauj lwm lawm

Txheej txheem cej luam ntawm Titanium tuav

 

Qeb 23 Kev Kho Mob Titanium Nqes yog cov hom khoom tshiab ntawm cov qauv khoom. Vim yog cov yam ntxwv ntawm titanium xws li siab lub zog, muaj zog heev, thiab kev ntxhov siab dhau los, thiab tsis muaj kev ntxhov siab nyob rau hauv cov cua sov thiab kev kub ntxhov. Nws tau thov nyob rau hauv high- Tech teb xws li kev lag luam zoo xws li kev tsim tawm, thiab yog cov khoom siv dej hiav txwv, thiab yam khoom siv txhua yam.

 

Cov lus qhia tshwj xeeb nyob rau qib 23 cov kab mob kho mob

 

Cov Khoom Siv Neeg Kho Tshuab

Teem nqi

Yam tseem ceeb

Tensile lub zog (RM / MPA) ntau dua lossis sib npaug

Tawm Lub Zog (RP0.2 / MPA)

Ntau dua los yog sib npaug

Elongation (%)

Ntau dua los yog sib npaug

Txo thaj chaw (Z%)

Ntau dua los yog sib npaug

TI-6AL-4V ELI

M

860

795

10

25

Qeb 5 (Ti-6al-4V)

M

860

780

10

/

 

Tshuaj lom neeg cov tshuaj lom neeg

Teem nqi

Ti

Al

V

FE,

tus zuag

C,

tus zuag

N,

tus zuag

H,

tus zuag

O,

tus zuag

TI-6AL-4V ELI

Tus liab

5.5~6.5

3.5~4.5

0.25

0.08

0.05

0.012

0.13

Qeb 5 (Ti-6al-4V)

Tus liab

5.5~6.75

3.5~4.5

0.3

0.08

0.05

0.015

0.2

 

Hais Txog Peb Lub Hoobkas

 

Baoji Reliab Hlau Khoom Co., Ltd yog lub chaw tsim tshuaj paus kev lag luam thiab cov khoom siv ntawm Titanium Zeb khoom thiab npib tsib xee, zirconium khoom. Nrog kev tswj hwm zoo, peb cov khoom tau ntsib tus qauv thoob ntiaj teb ua astm, ASCE, Forgys, thiab cov khoom siv thiab cov pob tw thiab CNC machined seem.

 

Tau 11 xyoos, Baeji Reliab hlau khoom tau cog ua ib qho ntawm cov neeg ua haujlwm ruaj khov rau ae} - qib titanium khoom nyob hauv Suav teb.

product-553-415

* Yuav tsum yog koj tus khub txhim khu kev qha thiab muaj peev xwm ntseeg tau ib txwm !! *

 

Cov ntawv thov ntawm Titanium tuav

 

* Kev kho mob

* Aerospace

* Aviation

* Caij nkoj

* Nkoj thiab kev ua rog

* Petrochemical kev lag luam

* Cov Khoom Siv Neeg Kho Tshuab

* Nuclear fais fab cuab yeej

* Cov Khoom Siv Hluav Taws Xob Hluav Taws Xob

* Cov tsheb thiab qhov chaw muaj tsheb

 

Cov duab qhia ntau ntxiv daim duab qhia ntawm qib 23 Titanium tuav

 

Grade 23 Medical Titanium Bars
Grade 23 Medical Titanium Bars in stocks
Grade 23 Medical Titanium Bars in low price
Grade 23 Medical Titanium Bars in high quality

 

Cim npe nrov: Qeb 23 Kev Kho Mob Cov Nqes Kho Mob, Suav Qeb, Suav Qeb 23 Kev Kho Mob Titanium tuav tuam ntxhab, lwm tus neeg, Hoobkas

Xa kev nug

(0/10)

clearall