Titanium alloys, raws li cov khoom siv hlau nrog kev ua tau zoo heev, yog siv dav hauv ntau thaj teb. Anodizing, raws li kev kho kom zoo rau cov khoom siv hluav taws xob, tuaj yeem coj mus rhaub peev xwm ntawm titanium alloys, nqa cov peev txheej tshiab rau kev txhim kho lawv cov kev ua tau zoo thiab nthuav lawv cov ntawv thov. Yog li, tuaj yeem titanium alloys yuav anodized? Cov lus teb yog muaj, thiab titanium alloy anodizing muaj pes tsawg tus cwj pwm tseem ceeb.
I. TSEEM CEEB LOJ UA NTEJ YUAV TSUM TAU TXAIS KEV ZOO
(I) Kev ua yeeb yam zoo heev: tom qab anodizing, oxide zaj duab xis tsim rau ntawm Titanium Alloy Deg muaj muaj kev ruaj khov tsis tshua muaj tshuaj. Nws corrosion tsis kam ntawm cov titanium alloy substrate, zoo tiv thaiv cov torrosion ntawm corrosion tshuaj, nyob rau ntau yam khoom siv lub neej. Piv txwv li, hauv ib puag ncig nrog cov accids muaj zog, hauv qab, Oxide zaj duab xis ua zoo li kev tiv thaiv loj "," muaj kev tiv thaiv zoo rau cov titanium alloy.
(II) Ntau haiv neeg tswj hwm: Los ntawm cov txheej txheem tswj kev haum, anodizing titanium alloys tuaj yeem ua tiav ntau yam ntawm cov txiaj ntsig zoo nkauj. Cov yeeb yaj kiab oxide tuaj yeem tso saib cov xim muaj xim muaj ntau yam, xws li kub, thiab liab doog xav tau cov kev thov kev zoo nkauj ntawm ntau yam kev siv. Qhov kev ua kom zoo nkauj no tsis yog ntxiv qhov kev thov tau pom tsis zoo rau cov khoom lag luam tab sis kuj nthuav tawm cov ntawv thov ntau yam kom zoo nkauj hauv cov chaw xws li kev kho kom zoo nkauj thiab cov hniav nyiaj hniav kub.
(III) Txhim kho saum npoo hardness thiab hnav tsis kam nce cov npoo tawv ntawm titanium alloys, mus txog ib qho nyuaj ntawm 300-800 hv. Tsis tas li ntawd, cov oxide zaj duab xis kev ua yeeb yam zoo hnav tsis kam, zoo tawm tsam sab nraud kev sib txhuam thiab kev puas tsuaj. Hauv kev siv cov tswv yim, cov khoom siv titanium alloy uas muaj undergone anlozing kev kho, xws li cov khoom siv kho tshuab thiab cuam tshuam, txo cov nqi siv.
Ii. Cov txheej txheem muaj zog hloov tau
(I) Muaj ntau yam kev xaiv electrolyte xaiv: titanium alloy anodizing kev kho muaj ntau cov electrolytes kom haum cov kev xav tau tshwj xeeb. Acidic electrolytes, xws li sulfuric acid thiab oxalic acid, tuaj yeem tsim cov yeeb yaj kiab oxalic nrog cov khoom tshwj xeeb thaum lub sijhawm kho; Alkaline electrolytes, xws li sodium hydroxide, tseem tuaj yeem muab cov kev cai tsim nyog rau oxide zaj duab xis tsim. Cov khoom sib txawv sib txawv muaj cov khoom sib txawv, cov qauv ntawm cov duab yeeb yaj kiab, yog li tau ntsib cov kev cai sib txawv.
(II) hloov pauv tau thiab hloov kho tau: Ntxiv rau kev xaiv ntawm electrolyte, thiab sijhawm) kuj tuaj yeem hloov kho kom tau raws li cov kev xav tau tshwj xeeb. Txawv parameter sib xyaw ua ke tuaj yeem ua rau kev hloov pauv hauv kev loj hlob tus nqi, tuab, thiab xim ntawm cov yeeb yaj kiab oxide. Piv txwv li, kev nce qib kev tsim nyog tuaj yeem nrawm qhov kev loj hlob ntawm cov oxide zaj duab xis, tab sis ntau dhau kev voltuage tuaj yeem ua rau txo cov yeeb yaj kiab zoo. Tswj qhov kub thiab sijhawm tso cai rau kev kho kho kom haum ntawm cov oxide zaj duab xis tuab thiab cov khoom kom tau raws li cov ntawv thov sib txawv.
(Iii) yoog tau rau ntau daim ntawv thov: Vim tias cov txheej txheem hloov tau, Titanium Alloy Anodizing, suav nrog kev kho mob, kev kho mob, thiab cov kev siv hniav. Hauv cov aviation teb, sulfuric acid system feem ntau yog siv rau kev ua kom muaj kev phom sij thiab hnav tsis kam ua rau muaj kev nyab xeeb hauv av; Hauv cov duab kho kom zoo nkauj, oxalic acid system yog siv kom ua tiav cov xim cuam tshuam los ntawm lub hauv paus kev cuam tshuam, ntxiv cov cim kos duab zoo nkauj rau kev dai kom zoo nkauj. Kev tshawb xyuas cov koom tes ua haujlwm tshiab tau taw qhia tias yog qhov yuav tsum tau ua rau cov khoom lag luam txuas ntxiv mus ntxiv, ua kom muaj kev ua tau zoo ntxiv thiab hauv {qhov tob.
Hauv cov ntsiab lus, titanium alloys tuaj yeem yog anodized, thiab cov kev kho mob no muaj cov yeeb yaj kiab tseem ceeb, thiab cov txheej txheem kev nthuav dav. Cov yam ntxwv no ua rau Titanium alloy anodizing kev kho mob muaj kev txhawb nqa cov kev pab cuam uas txhim kho thiab thov kev ua haujlwm ntawm cov alloys titanium.

Yog tias koj tab tom nrhiav rau titanium cov ntaub ntawv xws li Titanium daim hlau, tuav, xaim thiab titanium reliab hlau yog koj ib - nres muag khoom. Peb muab cov khoom lag luam zoo rau cov khoom lag luam zoo nrog cov khoom xa tuaj sai, thiab 24 {{{}} kev muag khoom thiab cov kev pabcuam tom qab muag.
Tiv tauj peb raws li cov ntaub ntawv hauv qab no:
Baeji Reliab Hlau Khoom Co., Ltd.
Tel: +86-917-8883215
Kev Muag Khoom Muag Khoom 1: +8613092900605 (mr.gary)
Muag Khoom Muag 2: +8613092913521 (ms. Sophia)
Chaw Nyob: No.35 Baoti Rd, Weibin District, Baoji, Suav