Cov txheej txheem kho saum npoo rau 3D- luam tawmtitanium rodsFeem ntau suav nrog cov hauv qab no, uas yog tsim los txhim kho lawv qhov zoo, cov khoom siv kho tshuab, thiab kev ua haujlwm:
I. Mechanical Polishing
1. Sandblasting: Siv cov abrasives xws li Al₂O₃ lossis iav hlaws dai kom sib npaug ntawm qhov chaw; haum rau kev kho mob ua ntej.
2. Vibratory / Sib Nqus Polishing: Haum rau qhov me me lossis cov txheej txheem nyuaj; zoo txhim kho nto tiav.
3. CNC Finishing: Milling los yog tig ntawm siab -precision mating nto los xyuas kom meej qhov ntev kam rau ua.
II. Tshuaj thiab Electrochemical Polishing
III. Cov txheej txheem Advanced
1. Chemical Polishing: Smooths saum npoo los ntawm cov tshuaj dissolution; tshwj xeeb tshaj yog tsim rau cov qauv ntxeem tau lossis cov kab noj hniav nyuaj, txo qhov roughness ntawm 6-12 μm mus rau 0.2-1 μm.
2. Electrolytic Polishing: Tsim los rau stainless hlau thiab titanium alloys, nws ho txhim kho nto tiav thiab tshem tawm oxidation nto.
Puab-Adaptive Sib Tsoo: Siv lub taub hau sib tsoo yooj yim kom txhuam tsis pub dawb- daim ntawv nto, ua tiav qhov roughness tsawg dua 10 nm.
Abrasive Flow Machining: Polishes sab hauv qhov chaw, qhov, kab noj hniav, thiab lwm yam nyuaj - mus rau - mus txog thaj chaw uas siv cov kua nplaum nplaum.
III. Kev kho mob ua haujlwm
Laser Polishing: Siv siab- lub zog lasers kom yaj cov nplaim, ua tiav qhov roughness ntawm 2-3 μm; Txawm li cas los xij, cov cuab yeej siv tau zoo heev.
Anodizing: Tsim cov oxide zaj duab xis ntawm titanium nto los txhim kho corrosion kuj, hardness, thiab hluav taws xob rwb thaiv tsev, thiab tso cai rau xim.
Phosphating: Ua hauj lwm raws li pretreatment rau txheej, txhim kho txheej adhesion thiab corrosion kuj.
Blackening: Tsim cov oxide zaj duab xis los tiv thaiv xeb; feem ntau siv rau qis- carbon steel, tab sis cov txheej txheem tshwj xeeb yuav tsum muaj rau cov titanium alloys. IV. Lwm yam technologies
Kub Isostatic Pressing (HIP): Seals nrog pores thiab txhim kho qhov ntom ntom; haum rau cov khoom siv nrog kev ua haujlwm siab.
Txheej / Plating: Xws li PVD txheej thiab anodizing los txhim kho hnav tsis kam lossis corrosion kuj.