1. Cov khoom siv sib piv
Ntshiab Titanium Tube: Qhov ceev 4.5g / cm³, qhov zoo dua qhov hnyav; nto oxide zaj duab xis yog tus kheej - kho, tiv taus cov kua qaub thiab alkalis.
316L Stainless Hlau: Ceev 8.0g / cm³, muaj cov nickel thiab molybdenum, tiv taus chloride ion corrosion tab sis yooj yim puas los ntawm cov concentrated hydrochloric acid.
2. Kev noj qab haus huv thiab kev nyab xeeb ntshiab
Titanium: Sensitization tus nqi tsuas yog 0.6%, tsis muaj kev pheej hmoo ntawm nickel leaching, kho mob ntawv pov thawj.
316L: Nickel tuaj yeem ua rau muaj kev tsis haum rau 15% ntawm cov pejxeem; Ntev - lub sij hawm raug tuaj yeem tso cov kab ntawm cov hlau ions.
3. Daim ntawv thov Scenarios
Pure Titanium Tube: Ib puag ncig tsis zoo xws li cov cuab yeej siv tshuaj, cov khoom siv tshawb nrhiav tob tob - hiav txwv, thiab kev cog qoob loo.
316L Stainless Hlau: Kev siv nyiaj txiag xws li kev kho vaj tse thiab khoom siv hauv tsev txhua hnub.
4. Tus nqi thiab kev ua haujlwm
Ntshiab Titanium: Cov khoom raug nqi ntau dua 15 npaug ntawm 316L; yuav tsum tau argon{2}}kev tiv thaiv vuam; tsawg ua efficiency.
316L: Yooj yim rau tshuab, tuaj yeem ua haujlwm nrog cov cuab yeej zoo tib yam, haum rau ntau lawm.
Nyob rau hauv cov ntsiab lus: ntshiab titanium tubing yog superior nyob rau hauv corrosion kuj thiab biocompatibility, tab sis yog kim dua; 316L stainless hlau muaj txiaj ntsig zoo rau cov nyiaj thiab tsim nyog rau cov kev xav tau dav dav.


Baoji Reliab Metal Materials Co., Ltd
Txawb: 0086 13092900605
Chaw Muag Khoom 1: WhatsApp +8613092900605 (Mr.Gary)
Chaw Muag Khoom 2: +8613092913521(Ms. Sophia)
Chaw nyob: No.35 Baoti Rd, Weibin District, Baoji, Suav