Lub zog titanium li cas?

Jul 05, 2025

Titanium Baryog ib qho ntawm cov muaj zog thiab cov hlau uas ruaj khov tshaj plaws, nrog lub zog tensile uas yog piv rau cov hlau ntawd.

Titanium bar yog siab tiv taus corrosion, txawm nyob rau ib puag ncig hnyav xws li cov dej hiav txwv lossis acidic ib puag ncig. Nws muaj lub siab yaj ntawm 3,000 degrees Fahrenheit, ua rau nws zoo tagnrho rau high- qhov kev thov kub.

Titanium bar tsis yog -} sib nqus, ua rau nws muaj txiaj ntsig hauv qhov uas hlau muaj kev cuam tshuam yog kev txhawj xeeb.

 

Peb paub ntau ntxiv txog Titanium tuav hauv qab no:

info-400-400

 

Ti6al4V titanium bar yog koom nrog titanium alloy thiab yog cov feem ntau cov titanium alloy hauv kev ua teb.

Titanium round bars yog cov feem ntau siv ntaus hauv cov khoom siv ua tau thiab nws tuaj yeem ua tiav rau ntau yam tshwj xeeb. Titanium alloy bar yog nrog tau zoo heev, corrosion tsis kam thiab muaj ntau yam muaj tseeb, tuaj yeem siv rau kev kho hniav thiab phais mob, ib qho kev phais mob thiab tsheb kho tsheb. Dhau li ntawm cov kab ke puag ncig, peb tuaj yeem muab cov kab tuav / cov pas nrig tau muab cov qauv ntawm cov duab tiaj, square bar, hex bar rau kev siv tshwj xeeb raws li Astm B348.

Tsis tas li, ntawm no yog kaum lub zog ntawm titanium bar:

1) Tsawg ntom ntom, lub zog muaj zog

2) Zoo heev corrosion corrosion

3) Cov cua sov tsis kam

4) Qhov kev ua tau zoo tsawg

5) muaj zog tiv thaiv damping kev ua tau zoo

6) Tsis {-} sib nqus, tsis yog - ua rau

7) Cov tshav kub me me conduction coefficient

8) cov qauv tsawg ntawm elasticity

9) Lub Sav Tsis Muaj Peev Xwm

10) tensile lub zog ze rau cov txiaj ntsig lub zog

Thiab peb tuaj yeem pom cov ntaub ntawv cov ntaub ntawv ntawm qib 5 titanium alloy bar:

Me me

Askiv

Hais lus

Cov Khoom Siv Lub Cev

Ceev

4.51g / cc

0.163 lb / Hauv³

Cov Khoom Siv Neeg Kho Tshuab

Hardness, Brinell

334

334

Kwv yees los ntawm Rockwellc

Hardness, Knoop

363

363

Kwv yees los ntawm Rockwellc

Hardness, Rockwell C

36

36

Tensile lub zog, qhov kawg

950 MPa

138000 psi

Tensile lub zog, tawm los

880 MPa

128000 psi

Elongation thaum so

14%

14%

Charpy cuam tshuam

17 J

12.5 ft - lb

V - imch

Los ntawm cov ntaub ntawv saum toj no, peb tuaj yeem pom tias Gr5 Titanium Alloy Cov tuav muaj lub zog siab, xeb tsis kam, qis}} kub ua tau zoo thiab lub teeb yuag. Thiab lub zog tensile ntawm gr5 titanium alloy bar yog ntau dua los yog sib npaug ntawm 825MPA, ua kom muaj kev sib luag rau 825MPA, ua kom muaj kev sib luag.

 