I. Mechanical Properties ofGr5 Titanium Square Bars
Lub zog siab - rau - qhov hnyav piv
Qhov ceev tsuas yog 4.43g / cm³, tensile zog 900-1100MPa, yield zog 850-1000MPa.
Siab -kub kev ua haujlwm ruaj khov: Tensile lub zog yog kwv yees li 900MPa ntawm 600 degree, thiab poob rau 650MPa ntawm 700℃.
2. Elastic modulus thiab hardness
Lub elastic modulus ntawm chav tsev kub yog 110-120 gpa, thiab nws txo qis me ntsis ntawm qhov kub thiab txias.
Vickers hardness: 330-400HV, Brinell hardness: 300-350HB.
Ii. Thermal Performance
1. Siab -kub tsis kam
Kev khiav hauj lwm kub yog -200℃mus rau 400 degree, thiab lub zog tensile tseem nyob li ntawm 700MPa nyob rau ntawm 500 degree.
Lub coefficient ntawm thermal expansion yog 8.5-9.5μm / m· degree, uas yog qis dua li ntawm aluminium alloy, thiab nws muaj qhov kub thiab txias qhov ntev.
2. Thermal conductivity thiab melting point
Thermal conductivity: 15-20W / m·K.
Melting point 1660-1680 degree, thiab nws cov oxidation kuj yog superior rau cov ntshiab titanium.
Iii. Corrosion kuj thiab biocompatibility
Nws muaj corrosion kuj zoo heev nyob rau hauv ntsev tsuag, dej hiav txwv thiab kua qaub- puag ncig puag ncig, thiab ib tug tsawg oxidation tus nqi nyob rau hauv 500 degree.
Zoo biocompatibility, dav siv nyob rau hauv orthopedic implants thiab kho hniav kho mob.
Iv. Txheej Txheem Txheej Txheem Technology
Forging : Qhov kub ntawm 900-950℃yuav tsum tau tswj kom tsis txhob tawg.
Kev kho cua sov: annealing optimizes toughness, thiab aging txhawb zog.
V. Cov ntawv thov ib txwm
Aerospace: cav Cheebtsam, fuselage yam ntxwv qhov chaw.
Kev lag luam tshuaj : corrosion-Reactors, pipelines .

Baoji Reliab Metal Materials Co., Ltd
Txawb: 0086 13092900605
Chaw Muag Khoom 1: WhatsApp +8613092900605 (Mr.Gary)
Chaw Muag Khoom 2: +8613092913521(Ms. Sophia)
Chaw nyob: No.35 Baoti Rd, Weibin District, Baoji, Suav