Titanium thiab titanium alloystseem tuaj yeem tswj lawv cov khoom ntiag tug ntawm cov khoom lag luam qis thiab ultra -} qis kub.
Raws li qhov ntsuas kub tsawg dua, lub zog ntawm titanium alloys tseem nce ntxiv, thaum lub ductility maj mam ua rau muaj kev txwv. Ntau cov annealed titanium alloys tseem muaj ducility txaus thiab pob txha lov nyuaj ntawm qhov kub ntawm 195,5 degrees. Cov uas muaj lub ntsiab tsawg heev cov ntsiab lus tuaj yeem siv tau ntawm qhov kub ntawm 252 degrees. Qhov sib piv ntawm nws cov ntsiab lus tsis muaj zog rau qhov tsis muaj zog tensile lub zog yog 0.95 ntawm qhov kub ntawm -25.7 degrees. Titanium alloys tseem tuaj yeem tuav qee yam khoom ntawm qhov kub. Kev lag luam feem ntau cov lag luam muaj peev xwm tswj hwm lawv cov peev xwm ntawm qhov kub ntawm 540 degrees, tab sis tsuas yog siv tau rau lub sijhawm luv. Qhov ntsuas kub ntau ntev rau lub sijhawm ntev yog 450-481 degrees. Titanium alloys rau siv ntawm qhov kub ntawm 600 tau tsim. Titanium alloys tuaj yeem siv ua cov ntawv sau npe ntawm qhov kub ntawm 540 degrees rau lub sijhawm ntev thiab ntawm qhov kub ntawm 760 degrees rau lub sijhawm luv.
1. Lub zog tensile ntawm ntshiab titanium yog 265-353 MPa, thaum twg ntawm cov annoys titanium yog 686-1176 MPa, tam sim no, tam sim no. Titanium alloys tau sib piv lub zog rau ntau cov qib titanium, tab sis titanium lub zog tshwj xeeb yog qhov qis dua li ntawm cov khoom siv titanium.
2. Lub zog compressive ntawm titanium thiab titanium alloys tsis tsawg dua li lawv lub zog tensile. Lub compressive thiab tensile tawm lub zog ntawm kev siv hluav taws xob ntshiab, thaum ti-6al-4V thiab Ti-5V thiab Ti-5V thiab Ti-5V thiab Ti-5V thiab Ti-5V thiab Ti-5Tsn muaj qhov ua tau zoo dua li tensile muaj zog dua li tensile muaj zog.
3. Shear lub zog yog feem ntau 60% -70% ntawm lub zog tensile. Lub compressive paib lub zog ntawm titanium thiab titanium alloy daim yog kwv yees li 1.2-2.0 lub zog tensile.
4. Nyob rau hauv ib txwm atighpheric muaj zog ntawm kev ua tiav thiab annaled titanium thiab titanium alloys yog 0.5-0.65 zaug lub tensile lub zog. Thaum raug mus rau 10 lab tus neeg qaug zog nyob rau hauv lub xeev nocles (Oct= 3.9}} {-v yog 0.2 lub sij hawm tensile lub zog.
5. Lub hardness ntawm high-}} Cov huab cua ntshiab titanium yog feem ntau tsawg dua 12,6- 295 HB. Lub hardness ntawm ntshiab titanium castings yog 200 - 220 hb. Lub hardness ntawm titanium alloys hauv annealed xeev yog 32-38 hrc (rockwell hardness), sib npaug rau 298-349 HB. Lub hardness ntawm li-cam khwb cia-5al-2.5SN thiab Ti20 HB yog 320 HB yog 320 HB, thaum lub hardness ntawm beterstitial Ti-6A1-4V casings yog 310 HB.
6. Lub tensile modulus ntawm industrial - ntshiab titanium yog 105 {}} 109 gpa. Feem ntau cov titanium alloys muaj tensile modulus ntawm 110 - 120 GPA hauv lub xeev annealed. Muaj hnub nyoog-hardened titanium alloys muaj me ntsis siab dua tensile ntau dua nyob rau hauv lub xeev annealed, thiab ntau dua cov modulus sib npaug los yog ntau dua cov modulus tensile. Qhov tshwj xeeb elastic modulus ntawm titanium alloys yog sib piv rau cov txhuas alloys thiab yog ob tsuas yog rau beryllium, molybdenum, thiab tej yam kev kub-alloys.
7. Nce cov ntsiab lus insterstwial los txhim kho lub zog ntawm titanium alloys tuaj yeem cuam tshuam rau alloy qhov cuam tshuam kuj thiab pob txha lov ceev. Nyob ntawm cov hom thiab lub xeev ntawm titanium alloy, lub charpy tsis cuam tshuam lub zog ntawm 15-54 j / m³, thaum lub xeev nrum nws yog kwv yees li 4-10 j / m³. Qhov cuam tshuam lub zog ntawm titanium alloys nyob rau hauv Anealed Xeev li ntawm 13-25.8 j / mg, nrog me ntsis qis dua nyob rau hauv lub xeev hnub nyoog.
8. Ntau lub titanium alloys muaj heev pob txha tawv, lossis, hauv lwm lo lus, ua tau zoo heev rau kev loj hlob tawg. Ti-6A1-4v Nyob rau hauv Annealed State yog cov khoom siv nrog cov khoom muaj zog zoo heev. Thaum lub ntsiab lus hais txog coeffici graini k=25.4 mm, qhov piv ntawm annate lub zog rau kev tawm dag zog tensile ntau dua 1.
Xaiv Baoji Reliab hlau rau koj cov khoom lag luam Titanium.
Yog tias koj tab tom nrhiav rau titanium cov ntaub ntawv xws li Titanium daim hlau, tuav, xaim thiab titanium reliab hlau yog koj ib - nres muag khoom. Peb muab cov khoom lag luam zoo rau cov khoom lag luam zoo nrog cov khoom xa tuaj sai, thiab 24 {{{}} kev muag khoom thiab cov kev pabcuam tom qab muag.
Tiv tauj peb raws li cov ntaub ntawv hauv qab no:
Baeji Reliab Hlau Khoom Co., Ltd.
Tel: +86-917-8883215
Txawb / WhatsApp: +8613092900605
+8613092913521
E - email: garychen3215@hotmail.com